Explain the one-bath and two-bath methods of leather tanning.
Operational Overview: Chrome tanning is generally carried out by two principal methods: the Two-Bath Method and the One-Bath Method. Currently, the one-bath method is strictly restricted or avoided because using hexaaquachromium(III) sulfate [[Cr(H2O)6]2(SO4)3] leads to elevated environmental effluent pollution. Among them, the two-bath method is more widely favored as it is both rapid and technically manageable.
In one-bath tanning, basic chromic sulfate is synthesized by reducing a sodium dichromate (Na2Cr2O7) solution using sulfur dioxide (SO2) or glucose:
The pickled hides are immersed directly in this chrome liquor bath containing common salt (NaCl) to prevent acid swelling. The hides are retained in the liquor for one night and then drained the next day. After 1 to 2 hours, the hides are transferred into a separate reduction drum containing a 15% sodium thiosulfate (Na2S2O3) solution. After remaining in this bath overnight, the hides are washed thoroughly with water, and borax is introduced into a settling drum to neutralize and diminish residual acidity. Following a final water rinse, the stock advances to the finishing operations.
Bated and pickled hides are loaded into a revolving tanning paddle. The chromium reagent and sulfuric acid (H2SO4) are batched relative to hide weight. Typically, for every 1 lb of hide weight, 5 lbs of a 2.5% – 3% solution composed of sodium dichromate [Na2Cr2O7 (5% – 6%)] and sulfuric acid [H2SO4 (33%)] are charged into the paddle.
The paddle is set into rotation and the hides are agitated for approximately 3 to 5 hours. Consequently, the hides absorb chromic acid, developing a uniform yellow color throughout their cross-section. At this stage, reactive collagen linkages become penetrated by Cr, forming an initial chromium-collagen intermediate complex.
The hides are subsequently lifted from the paddle, drained of surplus liquor, and transferred into a second paddle. This second bath contains a 6% – 10% working solution of sodium thiosulfate [Na2S2O3 (15% – 20%)] and hydrochloric acid [HCl (33%)]. Agitation continues, which reduces the hexavalent chromium to trivalent chromium, causing the yellow color to fade. Concentrated HCl is dosed gradually into the paddle until all yellow coloration is completely stripped away. This reduction cycle typically requires 24 to 48 hours to complete:
Finally, the hides are unloaded from the paddle and steeped in a glucose solution bath. This completely clarifies and reduces any trace residues of yellow chromate. Upon removal from the glucose bath and controlled drying, durable and finished Chrome Leather is obtained: